ENGINEERING DATA SHEET
CRYOGENICALLY TREATED VS. NITRIDED PUNCH AND DIE SET A-2 RC 60-62
Youngwood Electronic Metals West, a major metal fabricator for the electronics industry, needed a punch and die to form a 0.090 thick electronic iron material. The blank was 6” by 8” with a 90° form up with a leg off it at 84°. The die was designed to bottom and stipple two surfaces for part stability. The material used was A-2 Steel with a Rc hardness of 60-62. The deep cryogenically treated die was compared to a nitrided die.
THE CRYOGENICALLY TREATED DIE:
1. Lasted 200% longer with no signs of wear.
2. Could be reground. The nitrided die could not unless it was re-nitrided.
3. Maintained a #4 micro finish.
|
NITRIDED DIE |
CRYOGENICALLY TREATED |
|
|
Punch & Die Life |
- |
2X Longer |
|
#4 Micro Finish |
Worn |
Maintained |
|
Able to Redress |
No, not without re-nitriding |
Yes |